Assessment and management models of the built environment

Ecodesign in materials, construction systems and the built environment

Temporal flowability evolution of slag-based self-compacting concrete with recycled concrete aggregate

Authors:
Víctor Revilla-Cuesta, Marta Skaf, Amaia Santamaría, Jorge J. Hernández-Bagaces, Vanesa Ortega-López
Year:
2021
Journal:
Journal of Cleaner Production
Quartile:
Q1
Volume:
299
ISBN/ISSN:
0959-6526
DOI:
https://doi.org/10.1016/j.jclepro.2021.126890
Description:

<b>ABSTRACT</b></br>

The addition of by-products, such as recycled concrete aggregate and ground granulated blast furnace slag, modify the in-fresh flowability of ordinary self-compacting concrete both initially and over time. A detailed study is presented in this paper of 18 mixtures (SF3 slump-flow class) containing 100% coarse recycled concrete aggregate, two types of cement (CEM I or CEM III/A, the latter with 45% ground granulated blast furnace slag), different contents of fine recycled concrete aggregate (0, 50, or 100%), and three different aggregate powders (ultra-fine limestone powder <0.063 mm, limestone fines 0/0.5 mm, and recycled concrete aggregate 0/0.5 mm). The temporal evolution of slump flow, viscosity, and passing ability, and the values of segregation resistance, air content, fresh and hardened density, and compressive strength were evaluated in all the mixtures. The addition of fine recycled concrete aggregate and CEM III/A improved initial slump flow and passing ability by 6%, due to their higher proportion of fines. Nevertheless, the temporal loss of flowability within 60 min was 5.8% lower when adding natural aggregate and CEM I. Viscosity and air content increased 26% on average following additions of fine recycled concrete aggregate, unlike with additions of ground granulated blast furnace slag. Flowability and strength increased with the addition of limestone fines 0/0.5 mm. According to multi-criteria analyses, the mixtures with CEM III/A, 50% fine recycled concrete aggregate, and limestone fines 0/0.5 mm showed an optimal balance between their flowability (SF2 slump-flow class 60 min after the mixing process), compressive strengths (around 60 MPa), and carbon footprints.

</br>

<b>ACKNOWLEDGEMENTS</b></br>

This work was supported by the Spanish Ministry MCIU, AEI and ERDF [grant numbers FPU17/03374 and RTI 2018-097079-B-C31]; the Junta de Castilla y León (Regional Government) and ERDF [grant number UIC-231, BU119P17]; the Youth Employment Initiative (JCyL) and ESF [grant number UBU05B_1274]; the University of Burgos [grant number SUCONS, Y135. GI], UPV/EHU (PPGA20/26) and, finally, our thanks also to the Basque Government research group IT1314-19.